Regular in-service inspection is important to verify the integrity of welded nozzle sections in nuclear and other safety critical facilities. Nozzle sections made from austenitic steel can be susceptible to rapid crack growth due to thermal fatigue and stress corrosion. Early detection of cracks is therefore essential to ensure the continued safe operation of the facility in question. In order to ...